Monday, June 7, 2010

Re: [MW:5430] welding A335 P91 with Carbon steel

Hello Mauricio.
Looking for a electrode with similar element that the metal with more element and afther other PQR similar.
Review ASME IX and API 1104.
 
Agustin
 


De: mauricio padilla <mauricio_padilla_f@yahoo.com>
Para: materials-welding@googlegroups.com
Enviado: dom, junio 6, 2010 5:01:13 PM
Asunto: [MW:5416] welding A335 P91 with Carbon steel

Sirs,
 
I have a question about welding dissimilar material:
 
One Metal:          A335 P91 ----------------------------------        PNumber 15E
Second Metal      MSS SP75 WPHY-70  ---------------        Snumber 1
 
Wall thickness                                                              36.53 mm
 
Which ones are the best  FILLER METAL for   GTAW?
 
Which ones are the best  FILLER METAL for   SMAW?
 
 
Is it necessary PWHT?
 
Please give a tips.
 
Best Regards
 
Mauricio

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

 

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...