Re: [MW:5405] storage condition of E6013

Dear Mr.M. Sagukumar,
 
 As per my experience the redrying  or backing  temperature for E-6013 electrode is 90-100 o'Celcius. Not more than that it will loosen the coating.These are not the Low Hydrogen electrodes.
 
 
 
PANKAJ


 
On Sat, Jun 5, 2010 at 2:51 PM, sugu puma <pumamy@yahoo.com> wrote:
Dear all,
The baking temperature is 350 - holding temperature 150,see the manufacture rules and regulations before open the box of electrode cartoon,this is all low hydrogen electrode using,followup according manufacture recommendation and also take look in AWS D1.1.

From,
M.Sugumar


From: Sandeep Kp <sandeepkp99@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Sat, June 5, 2010 10:34:30 PM
Subject: [MW:5401] storage condition of E6013

Dear all,
Let me know the baking & holding temperature of E6013 electrodes of ESAB.
 
 
Regds,
 
Sandeep.k.p
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...