Mr. KK,
Good evening,
If you want to use wire type IQI as per ASME Sec. V, please refer to Article 2, table T-276.
Further to decide which set to select, refer table T-233.2
Please note that you have to consider the weld reinforcement as per referencing code, in order to select IQI.
Hope this will clarfy.
Regards.
John Rodrigues,
Al Shabia Engg. Co. Ltd.
Sharjah, UAE.


On Sat, 05 Jun 2010 18:46:04 +0530 wrote
>Guys,
>
Can anyone send me the IQI chart wire type as per the ASME/ISO Standards.
>

>
kk




--
>
To post to this group, send email to materials-welding@googlegroups.com
>
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
>
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
>
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>



John Rodrigues

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...