Hi Mr. Tamer
 
RT is not required but if you take RT you can avoid the defect while preparing the specimen for destructive testing or you can make a new sample for destructive testing.
 
Best Regards.
Manoj


 
On Tue, Jun 1, 2010 at 10:08 AM, tamer said <tamer_bajio@yahoo.com> wrote:
Dear all,
For welding procedure qualification (PQR) as per API 1104, is it required radiographic testing with destructive testing or no ???
Tamer Said
QA/QC Engineer
Kuwait




--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...