Hi,
     Refer Table T-276 of ASME Sec-V to identify the Hole and Wire type IQI.
Also you can calculate the Thickness of wire by the following formula.
% IQI Sensitivity =  Thickness of the thinnest wire visible
                            ------------------------------------------------------ * 100
                              Object Thickness 

Regards,
Vaithiyanathan,
QA Engineer,
Worleyparsons Arabian Industries 
Oman.


On Mon, May 31, 2010 at 2:57 PM, Subrata Das <sdas@pkgroup.org> wrote:

Dear All

My job is Carbon steel and thickness is 20 mm. For radiography I have to select the IQI set as material group as "1" and wire type set as "A or B or C or D". Can you please guide me how to select the set identification number based on thickness of job.

 

Thanks in advance

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With Best Regards

B.Vaithiyanathan

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...