You use 2% he mixture in the argon welding gas to get a better penetration or fusion.

Regards, jimmy

On 10 Jun 2010 09:36, "Kathalingam Babu" <kathalingam.qaqc@ppl.com.sg> wrote:
> Hi
>
> It is the one upcoming process in india, still research is going at IGCAR , kALPAKKAM by Mr.Vasudevan .
>
> I remember that , when i was doing my master thesis under Mr.Vasudevan of IGCAR KALPAKKAM, he has involved A-TIG research & Holding the patent for this process in india.
>
> If any body want more details about this process, you can contact him for the further details.
>
> Regards,
>
> K.Babu
> Singapore.
>
>
> ----- Original Message -----
> From: Bathula Raghuram (Mumbai - PIPING)
> To: 'materials-welding@googlegroups.com'
> Sent: Wednesday, June 09, 2010 6:40 PM
> Subject: RE: [MW:5487] Active TIG?
>
>
> Further to below pl. refer attachment
>
>
>
> --------------------------------------------------------------------------------
> From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pankaj abhang
> Sent: Wednesday, June 09, 2010 3:40 PM
> To: materials-welding@googlegroups.com
> Subject: Re: [MW:5486] Active TIG?
>
>
>
> Dear kesavalunanda,
>
> Active-TIG welding ( hereinafter called as A-TIG welding ) is a welding method capable of drastically increasing further its penetration depth than in the conventional TIG welding by applying an active flux on the surface of steel product placed on the welding line. This welding method was proposed in 1960's, and is practically applied so that it can be easily used by the progress of recent research and development. By this, a drastic efficiency improvement can be materialized in TlG welding, drawing remarkable attention to it. which is such a new welding method.welding.
>
>
>
> Regards,
>
> Pankaj
>
> On Mon, Jun 7, 2010 at 8:42 PM, kesavalunanda <kesavalunanda@yahoo.co.in> wrote:
>
> Dear Friends,
>
> Can anybody clarify my doubt..please,
>
> the question is" what is A -TIG (Active-TIG) ?"
>
> This question is asked in AMIIW(Associate membership in Indian Institute of Welding-kolkata-www.iiwindia.com) Exam-Summer-2009(AME-15)
>
> Thanks,
>
> Regards,
>
> K.NANDAGOPAL ;
>
> +91 9698997022
>
> +91 9360049258-
>
> Tamilnadu,
>
> INDIA
>
>
>
>
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...