As per material requisition of one of our client says PWHT to be done regardless of thickness for Carbon Steel welded fittings. Can we go for Normalizing instead of PWHT after completion of forming as well as welding?
Thanks
Subrata
S355 J2 WP is a weathering structural steel It has better atmospheric corrosion resistance. Use E 8018 - W1/W2 Electrodes This is regular...