Thursday, June 17, 2010

[MW:5635] Maximum Angle of Inclination of 5G position

Dear all,
 
I have an query that we are doing pipeline welding that , during the road crossing section we could not achive exact  horizontal  position (ie 5G ).. the angle of inclination is 20 degree from horizontal plane.. what will be the maximum angle of inclination that we can weld in 5G position..
 
There is no specific position graphics in API 1104 like ASME BPV SEC IX...
 
Regards,
 
Mubarak.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...