This depends on what exactly you mean. Is there a specific QW-410.# to
which you are referring? The only sections of QW-410 that I can find
that reference oscillation or weaving are .1 and .7
QW-410.1 says "For manual or semiautomatic welding, a change from the
stringer bead technique to the weave bead technique or vice versa."
QW-410.7 says "For the machine or automatic welding process, a change
in width, frequency, or dwell time of oscillation technique."

Through my education I have learned that oscillation usually refers to
a circular motion, while weave refers to a back-and-forth motion.

This is as I know with which to answer your question, to be able to
answer you more fully would require more information.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34920] Tubesheet Hole step

Hello Team, I have one question any tolerance given for tubesheet Hole step. Please do needful. Regards, AP  -- https://materials-...