hi tamer
radiography is not so essential because ur welder gets qualified only
after the results of destructive testing only but if u take rt then u
can select the section for destructive testing or make a new specimen
for the destructive testing

On Jun 1, 2:08 pm, tamer said <tamer_ba...@yahoo.com> wrote:
> Dear all,
> For welding procedure qualification (PQR) as per API 1104, is it required radiographic testing with destructive testing or no ???
> Tamer Said
> QA/QC Engineer
> Kuwait

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34919] Welder qualification certificate

Dear All     anyone can share a format for welder certificate and card format        Thanks & Best Regards Saleem manhappulath Mob:+9665...