Hi There,
Our welder is qualified to weld CUNI on a 6G position 40mm diameter (test coupon size on PQR) as per ASME IX qualification. My question is, is he also qualified to weld a CUNI 20mm diameter tube using the same WPS?
Cheers,
Larry Zarate
S355 J2 WP is a weathering structural steel It has better atmospheric corrosion resistance. Use E 8018 - W1/W2 Electrodes This is regular...