Present here the basic differences between the Two Materials.
A 351/A 351M – Standard Specification for Castings, Austenitic, Austenitic-Ferritic (Duplex), for Pressure-Containing Parts
A 743/A 743M –Standard Specification for Castings, Iron-Chromium, Iron-Chromium-Nickel, Corrosion Resistant, for General Application
Grade, Type, Carbon max, Manganese max, Silicon max, Phosphorus max, Sulfur max, Chromium, Nickel, Molybdenum
A743/CF3M, 0.03, 1.50, 1.50, 0.04, 0.04, 17.0–21.0, 9.0-13.0, 2.0–3.0,
19 Chromium 10 Nickel, with Molybdenum,
A351/ CF3M 0.03, 1.50, 1.50, 0.04, 0.04, 17.0–21.0, 9.0-13.0, 2.0–3.0,
Regards.
Bagesh Kumar
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Darji Nilesh (Mumbai - Machinery)
Sent: Friday, March 05, 2010 2:28 PM
To: materials-welding@googlegroups.com
Subject: [MW:4430] Material Properties :
- A 351 CF3M
- A 743 CF3M
Both material grades are for Casting. Requirement is for Pump Impeller in SS 316LCast Material.
What is the diff. between above TWO Materials.