Wednesday, March 3, 2010

[MW:4407] evaluating based on AWS D1.1 for UT

Dear All
what is the sensitivity refrence line for ultrasonic testing according AWS D1.1?
is DAC applicable?(if yes, in which paragraph this refered?)
regards

1 comment:

Unknown said...

AWS D1.1 Does not allow the use of DAC. AWS is strictly based on the defect points system. I appologize as I do not have the code near me at the moment but I have dealt with this issue a number of times.

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...