Re: [MW:4301] Interpass temperature

Hi,
As close to the weld and heat affected zone as practicable would be the appropriate approach as we are interested in controlling metallurgical transformations in the previous weld pass and HAZ.
Shashank

--- On Fri, 12/2/10, Dindo <dindodelacruz@gmail.com> wrote:

From: Dindo <dindodelacruz@gmail.com>
Subject: Re: [MW:4292] Interpass temperature
To: materials-welding@googlegroups.com
Date: Friday, 12 February, 2010, 7:56 PM

you coul either use a tempilstik of a thermoscanner
 


 
On Fri, Feb 12, 2010 at 7:24 AM, Dindo <dindodelacruz@gmail.com> wrote:
it all depends on what the customer specify, It usually is measured 50 to 75mm from the edge of the bevel, that's how we do it on pipelay
 


 
On Thu, Feb 11, 2010 at 12:37 PM, Jamie Welding <jamesmathewtrading@gmail.com> wrote:
As per ASME sec 9 definition interpass temperature is the temperature
measured just before the start of next pass.So where is it to be
measured.
On the weld pass before start of the next pass.But this is very
impracticable.
Can anyone suggest.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Your Mail works best with the New Yahoo Optimized IE8. Get it NOW!.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...