Thursday, February 25, 2010

Re: [MW:4373] Robot - WOPQ?

Dear Prem,
Operator qualification is required.
 
Regards,
Ibrahim

On 25 February 2010 16:05, PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com> wrote:
Dear All

We have a typical situation.
We want to do overlay by FCAW and want to deploy robot for this i.e by automatic welding.
The construction code is ASME Sec VIII Div.1

Now as per ASME Sec VIII Div1, UW29(b)(2)-- "when welding is done by any automatic welding process, performance qualification testing is not required".
So do we need not do any WOPQ ?? Is performance qualification required or not ??
Pls.. advise..

Regards

Prem Nautiyal

PREM S NAUTIYAL
CELL : 9820313278

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks & Regards
Muhammed Ibrahim PK

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...