Dear All, We are working on PQR & deatails are as folows : Appl. Code - DNV OS F101,2000 PQR - Through THickness Repair. (SMAW) Base Metal - API 5L X GRADE 60 - 12.75" OD X 14.3 mm THK. Filler Metal - E-7018 H4R Position -6G After mechanical tests, we are getting all values in acceptable limits except All Weld Tensile results.(Reqd- 517 Mpa & Actual - 483 / 493 Mpa) What is the reason & solution for the same? Pl. reply. PSP |