Hi,
F No. is 6. No P no. for consumables. P no. is for materials.
Thanks,
K.Rajagopal

On Fri, Feb 26, 2010 at 9:27 AM, Arshad Farooq Syed <arshad_farooq64@yahoo.com> wrote:
kindly advise me regarding the F NO AND P NO FOR ER-309L
 
 

Regards

 

Syed Arshad Farooq 

 QA / QC Engineer

 PROCTER & GAMBLE

 D.L UNIT KARACHI

(+92-21-111-284-284,5378637-40

): +92-308-3067599


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...