[MW:4380] ferrite number of duplex stainless steel weld

Hi,
We have a different understanding for the generally, the oil & gas industry, the percent ferrite should be between 35 - 60% and the FN from 4 - 8

We would assume you are using Ferritscope MP 30 for the measurement


David Chan
~~~~~~~~~~~~~~~~~~~~~~~~~~
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Sukamal Naskar
Sent: Friday, February 26, 2010 1:22 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:4376] ferrite number of duplex stainless steel weld

Optimum is 50FN, but 40 ~ 70 FN will be acceptable , but still it
depends on the client's technical specifications.

Regards,

On 2/26/10, pankaj.johri@in.transport.bombardier.com
<pankaj.johri@in.transport.bombardier.com> wrote:
> Hi,
>
> We are welding duplex stainless steel.
>
> To control the parameters of welding, we are measuring ferrite number of
> weld.
>
> Can anybody tell us how acceptable values of ferrite numbers are decided.
>
>
> Regards,
>
> Pankaj
>
>
> Please consider the environment before you print / Merci de penser à
> l'environnement avant d'imprimer
>
> _______________________________________________________________________________________________________________
>
> This e-mail communication (and any attachment/s) may contain confidential
> or privileged information and is intended only for the individual(s) or
> entity named above and to others who have been specifically authorized to
> receive it. If you are not the intended recipient, please do not read,
> copy, use or disclose the contents of this communication to others. Please
> notify the sender that you have received this e-mail in error by reply
> e-mail, and delete the e-mail subsequently. Please note that in order to
> protect the security of our information systems an AntiSPAM solution is in
> use and will browse through incoming emails.
> Thank you.
> _________________________________________________________________________________________________________________
>
>
> Ce message (ainsi que le(s) fichier(s)), transmis par courriel, peut
> contenir des renseignements confidentiels ou protégés et est destiné à
> l?usage exclusif du destinataire ci-dessus. Toute autre personne est, par
> les présentes, avisée qu?il est strictement interdit de le diffuser, le
> distribuer ou le reproduire. Si vous l?avez reçu par inadvertance,
> veuillez nous en aviser et détruire ce message. Veuillez prendre note
> qu'une solution antipollupostage (AntiSPAM) est utilisée afin d'assurer la
> sécurité de nos systèmes d'information et qu'elle furètera les courriels
> entrants.
> Merci.
> _________________________________________________________________________________________________________________
>
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>


--
Sukamal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...