[MW:4129] RE: 4123] Demagnetization after completion of MPI test

Dear Mr Raghavendra,

The attached ASTM spec(Clause-12) provides brief introduction on demagnetization. From my experiences I have seen that AC magnetic coils can induce a lot less of residual magnetism thatn DC coils. PWHT effectively nullifies residual magnetism as the temperature very close to curie point.

If you have any specific recomemnedations from your client feel free to share the same.I am not posting this ASTM document in the forum due to copyright issues.

Earler I had sent you some information on Reheat cracking in Cr-Mo-V steel welds with SAW welding. Did it fit well into your information requirements. Appreeciating your response.

Thanks

Pradip Goswami, P.Eng
88,Garth Trails Crescent
Hamilton,Ontario, L9B2X1,Canada
Email-pgoswami@sympatico.ca
Email-pgoswami@quickclic.net


-----Original Message-----
From: materials-welding@googlegroups.com [
mailto:materials-welding@googlegroups.com
] On Behalf Of PEMMARAJU RAGHAVENDRA
Sent: Thursday, January 21, 2010 7:24 AM
To: materials-welding@googlegroups.com
Subject: [MW:4123] Demagnetization after completion of MPI test

Dear All,

Can any one tell us the various methods / procedure  of demagnetizing the weld after completion of Magnetic particle testing on Ferritic steel welds.

Regards,

Raghavendra 

Larsen & Toubro Limited
www.larsentoubro.com

This Email may contain confidential or privileged information for the intended recipient (s) If you are not the intended recipient, please do not use or disseminate the information, notify the sender and delete it from your system.


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...