[MW:4336] RE: 4335] PWHT OF MATERIAL P No.5B

Pl. indicate complete material specification (is it P5A, P5B and which group number?)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of John Manoj
Sent: Wednesday, February 17, 2010 8:02 PM
To: materials-welding@googlegroups.com
Subject: [MW:4335] PWHT OF MATERIAL P No.5B
Dear all,

I need the following information. 

what is the soaking temperature?
what is the minimum holding time? 
What is the preheat and interpass temperature?

i have to make 1" sch 80 SA 335 Gr. P5  coil and there are 5 butt joints and i have to qualify wps aslo as per ASME SEC. IX.
As per ASME SEc. VIII Div. I normal holding temp. is 675 degree C and minimum holding time is 15 minutes. 
and as per ASME SEC. II part C Holding temp. is 745 degree C and holding time  is 1 hr./ in.

Thanks & Best Regards.

Manoj.


No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...