[MW:4375] ferrite number of duplex stainless steel weld
Hi,
We are welding duplex stainless steel.
To control the parameters of welding, we are measuring ferrite number of weld.
Can anybody tell us how acceptable values of ferrite numbers are decided.
Regards,
Pankaj
Please consider the environment before you print / Merci de penser à l'environnement avant d'imprimer
_______________________________________________________________________________________________________________
This e-mail communication (and any attachment/s) may contain confidential or privileged information and is intended only for the individual(s) or entity named above and to others who have been specifically authorized to receive it. If you are not the intended recipient, please do not read, copy, use or disclose the contents of this communication to others. Please notify the sender that you have received this e-mail in error by reply e-mail, and delete the e-mail subsequently. Please note that in order to protect the security of our information systems an AntiSPAM solution is in use and will browse through incoming emails.
Thank you.
_________________________________________________________________________________________________________________
Ce message (ainsi que le(s) fichier(s)), transmis par courriel, peut contenir des renseignements confidentiels ou protégés et est destiné à l’usage exclusif du destinataire ci-dessus. Toute autre personne est, par les présentes, avisée qu’il est strictement interdit de le diffuser, le distribuer ou le reproduire. Si vous l’avez reçu par inadvertance, veuillez nous en aviser et détruire ce message. Veuillez prendre note qu'une solution antipollupostage (AntiSPAM) est utilisée afin d'assurer la sécurité de nos systèmes d'information et qu'elle furètera les courriels entrants.
Merci.
_________________________________________________________________________________________________________________
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...