Friday, February 26, 2010

[MW:4379] RE: 4377] F NO AND A NO FOR ER-309L

F#6 and A#8, P no is applicable only for base material (P#8 for 300 series ASS)


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Arshad Farooq Syed
Sent: Friday, February 26, 2010 10:57 AM
To: materials-welding@googlegroups.com
Subject: [MW:4377] proposed wps

kindly advise me regarding the F NO AND P NO FOR ER-309L
 
Regards

Syed Arshad Farooq 

 QA / QC Engineer

 PROCTER & GAMBLE

 D.L UNIT KARACHI

(+92-21-111-284-284,5378637-40