Re: [MW:4310] AFFECT POLARITY IN HEAT INPUT

Yes because when the electrons flow to the electrode the base metal is heated less


  From: ali asghari [asgharialigl@gmail.com]
  Sent: 13/02/2010 07:59 ZE3B
  To: materials-welding@googlegroups.com
  Subject: Re: [MW:4297] AFFECT POLARITY IN HEAT INPUT


thank you
but my inyention is distribution of heat is differed by polarity , therefore H.I depend to polarity.is it true?
regards

On Sat, Feb 13, 2010 at 2:04 AM, <george.dilintas@gr.bureauveritas.com> wrote:

It is because of the difference of the electrons flow I think


  From: Ali Asghari [asghariali@rocketmail.com]
  Sent: 11/02/2010 23:44 PST
  To: materials-welding@googlegroups.com
  Subject: [MW:4291] AFFECT POLARITY IN HEAT INPUT


Hi All
all know that heat input is independent from polarity.but  i see in GTAW that in DCEN ,70%HEAT generated in arc concentrated in parent metal & in DCEP 30% HEAT concentrated in base metal.
can anybody clarify it?
regards.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...