Dear Israr Ahmed
my base metals are S355K2G3 & S355NL

On 2/16/10, israr <ahmedisrar.nm@gmail.com> wrote:
> Dear Ali Asgari,
>
> Pls ref material Specification ASME Section II, Every material has
> specified some impact value at diffrent tempreture.
>
> Or Tell me the material specification which you are going to weld.
>
>
> Regards
>
> Israr Ahmed
> +966530417332
>
> On Feb 14, 11:21 am, Ali Asghari <asghari...@rocketmail.com> wrote:
>> Hi all
>> i want to weld to pipe steel that have simillar tensile strength, but they
>> have simillar impact toughness in different temp(-20&-40).
>> now for qualification of this weld, how can i assess temp in which impact
>> samples tested?
>> is in any standard or code specified rules to weld dissimillar steels in
>> toughness?
>> regards.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding-unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...