Thursday, February 18, 2010

[MW:4339] Fwd: Querry regarding the PWHT



---------- Forwarded message ----------
From: Sameer Wakde <smwakde@gmail.com>
Date: Thu, Feb 18, 2010 at 10:51 AM
Subject: Querry regarding the PWHT
To: MANOHAR BEHARA <beharamanohar@gmail.com>, Sudheer Babu <sudheerbabun@gmail.com>, 

Dear Sir

Good morning. I want your help in the following matter

We are doing the CWS/CWR line having dia from 80" ~ 112" & thickness over 20 mm upto 28.58 mm O.P 5.5 Kg/Cm2.

We are carrying PWHT due to the thickness requirement, but we want to deviate as the para 331.2.2 of B31.3. So if anybody have qualified WPS without PWHT in such cases, please guide me & send the WPS for the reference purpose.

With warm regards

--
Sameer Wakde
DFCU & AU PROJECT
SAMSUNG Engineering
Bharuch, India
+91 9714349279

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...