Thank you Dr. G. Dilintas for reply.

I would like to clarify that,

This shell is not offered to QA/QC so far. This issue is with production only right now.
So, do you mean that internal NCR to be raised by manufacturer himself ?

Can you elaborate on mock-up thing ?

NDT of seams are balance and it will be tested by 100% MT+TOFD.

Is this a weld-repair ?

Regards,
Krissy


On Tue, Feb 16, 2010 at 5:26 PM, <george.dilintas@gr.bureauveritas.com> wrote:

It is not a good practice but the code (ASME VIII-1) does not prohibit repairs in general.
If you have done spot radiography then you have to take care about additional RT increments.
It is an NCR since you have affected the out of roundness.
I would suggest to make a mock-up first

Dr. G. Dilintas
I&F Regional Technical Manager
Bureau Veritas Piraeus - Greece
Tel: +30 210 40 63 113/4
Fax: +30 210 40 63 118
Inactive hide details for Krissy D <krissy.diva@gmail.com>Krissy D <krissy.diva@gmail.com>




To

materials-welding@googlegroups.com

cc


Subject

[MW:4323] Re-welding of completed weld joint

Ref


Posting a query from a Message Board:

Good Morning Everybody,

We have following situation during fabrication of a pressure vessel :

There are 3 Long seams in a fabricated Shell section.
Welding of all 3 seams are completed and
all NDT are balance for these seams.
There are some stringent dimensional requirements as per client's specification. Due to high thickness, significant distortion (peak-in/out) had occurred. Now production people is planning to correct it. For that, they have removed some 50% of one side of weld in one particular joint by grinding. And planned to re-weld it to negate the distortion effect.

Shell material is SA387 Gr 11 Cl 2 with SA 240 Type 410S cladding having thickness of 44.5+4.5 mm.
Pre-heating, Interpass Temp., DHT & ISR/PWHT are required as per WPS.

Now my question is
(1) Is it allowed as per general engineering practice of pressure vessel fabrication ?
(2) Can I call it a repair and can use WPS of weld-repair ?
(3) Is it a case of NCR ?
(4) Is it acceptable as per Code ?

Please suggest your views on this.

Regards,

Krissy

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...