We are executing a job in a cement plant for reconditioning of LS crusher primary rotor. All the ribs got worn out upto 80mm and need a build up of 80mm with final layer of hardfacing. We have recommended the following combiniation for the said job.
 
1. Cushioning layer :Alloy Base Fe, Cr, Mn, Ni which is highly wrok hardening in service.High resistance to impact and deformation
 
2. Build up:  Ally base Cr, Mn, C, Fe which is tough austenitic managanese based steel welding alloy to resist high impact
 
3.Hardfacing: Alloy base: Fe, Cr, Mn which is resistant to low stress scratchiing and high stress grinding abrasion.
 
Now our colleagues have welded one phase using a single buffer layer and and build up upto 80 mm completely with the electrode without using any ms plate. The job got cracked and the crack was opened up to 10 to 15 mm width.
 
Kindly let me know how to repair the crack without spoiling the build up much and how to carry the rest three phases.
 
Please advice and suggest, your quciker reply helps me a lot.
 
Best Regards
 
G.Srinivas


The INTERNET now has a personality. YOURS! See your Yahoo! Homepage.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...