[MW:4325] Re: different impact toughness

Dear Ali Asgari,

Pls ref material Specification ASME Section II, Every material has
specified some impact value at diffrent tempreture.

Or Tell me the material specification which you are going to weld.


Regards

Israr Ahmed
+966530417332

On Feb 14, 11:21 am, Ali Asghari <asghari...@rocketmail.com> wrote:
> Hi all
> i want to weld to pipe steel that have simillar tensile strength, but they have simillar impact toughness in different temp(-20&-40).
> now for qualification of this weld, how can i assess temp in which impact samples tested?
> is in any standard or code specified rules to weld dissimillar steels in toughness?
> regards. 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...