This specification covers recommended procedures for the tube end welding of tubes ranging from ½ in (15 mm) to 1½ in (40 mm) nominal diameter and from 1.6 mm to 4.1 mm wall thickness to tube plates of 15 mm and over, in ferritic and austenitic materials.

it covers materials, design, PQR, strength tests, leak testing, expansion etc.

On Sat, Feb 27, 2010 at 1:30 PM, Praphulla <praphulla.dp@gmail.com> wrote:
Dear All,
Can anyone help me to understand the requirements of EEUMA 143?
Do you have any reference article of EEUMA 143?
 
Thanks
Praphulla

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...