Monday, February 1, 2010

[MW:4169] how to conduct moly test? to differentiate SS304/SS316

dear members,
i would like to conduct moly test to differentiate 304 vs 316.
please advise, where can i get those chemicals to perform the test.
Expert advise needed
regards,
Suresh.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...