[MW:3611] Re: PQR for 516 Gr60- HIC material

The consumable used for the same should report the HIC properties in
the Test Certificate.

Jaspal Singh

On Oct 29, 3:08 pm, "yusufkhan.pat...@gmail.com"
<yusufkhan.pat...@gmail.com> wrote:
> Dear all,
>
> I need to make a PQR for 516 Gr 60N-HIC material for thickness ranging
> from 10mm to 32mm with PWHT.
> Please suggest me what additional tests are required for HIC(Hydrogen
> Induced Cracking) material for the PQR along with Physical & Chemical
> Tests.
>
> Thanks in advance.
>
> Regards.
> Yusufkhan

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...