Wednesday, July 29, 2009

[MW:2845] Re: NACE compliant materail


HI,
     If the H2S increses then heavy corrosion will start , the material used will corrode very fast, maily valves, elbows, fittings... etc. weld joints etc.... The entire system can fail within a year or 6 months ....
On Wed, Jul 29, 2009 at 2:34 PM, Yadav Shiva <luvshiv2002@gmail.com> wrote:
Hi Srini,
               Use material with 18% Cr. for existing facilities, the problem is with client . You just go according to your requirment meets the NACE std. Dont worry about if it exceeds 10% or 20%........ if you wana to become scientest then its your coice.... enjoy.........
 
Y.C.Shiva,
QA/QC Engineer,
Doha Qatar.

On Tue, Jul 28, 2009 at 2:25 PM, Hari Srinivasa Murthy <harimurthy@gmail.com> wrote:
An Oil and Gas exploration gas processing facility has been designed for 3% H2S in the gas (NACE compliant material used in the existing facility). As we cannot predict the behavious of oil wells some times H2S content may increase. 
 
Please putdown your opinions on what could be the various implecations to plant equipment (materials)  if the H2S % raises to 8% or 9%. 
 
Regards
 
Srinivas 





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...