Monday, July 27, 2009

[MW:2818] Re: 2805] Inconel 600

Hi,

 

Check www.specialmetals.com on details on Inconel 600, and www.specialmetalswelding.com  click joining brochure to know more about welding of ni-base-alloys

 

Regards,

 

Marco

 

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PB HEGDE
Sent: 25 July 2009 08:30
To: materials-welding@googlegroups.com
Subject: [MW:2806] RE: 2805] Inconel 600

 

Hi!

For Inconel 600 matching consumables are

SMAW-ENiCrFe3

ii)TIG-ERNiCr3 with Nuclear grade Argon with ,Proper purging  , Use of Pulse tig ,with lower heat input will be able to produce good weld.

iii) I had experience of using Incoalloy  filler w/o any problem

iv) I have bad experience of using Mig process  hence can not share my experience

 

Other wise with good engg practices , not much problem of handling Inconel 600

 

Regards

 

Hegde

 

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of sorin stefan
Sent: Friday, July 24, 2009 8:06 PM
To: materials-welding@googlegroups.com
Subject: [MW:2805] Inconel 600

 


Hi Guys,
 
Please tell me what is the best match of the filer material and gas for welding ALLOY 600 ( plates 1/4"up to3/") using MIG and TIG procedures.
If you also have some welding giudelines - welding procedure regardless, it will be great
Getting an answer ASAP it will be very much apreciated
 
Thanks a lot
Sorin St.

 


Stay on top of things, check email from other accounts! Check it out.

 


lang=EN-US>


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...