[MW:2813] Re: LTCS Welding

MDMT for Ammonia service is normally below -30 degree centigrade , as you are using A333GR6 Materials which are normally certified for -46Degree centigrade , you use GTAW using ER70S2 Filler wire with impact tested propoerities -46degree centigrade  and rest welding using E 7018-1

Best Regards,


----- Original Message -----
From: Nikhil
To: materials-welding@googlegroups.com
Sent: Sat, 25 Jul 2009 10:52:20 +0530 (IST)
Subject: [MW:2807] LTCS Welding

Dear Friends,



I like to know whether we can use the combination of E6010 in root and E7018-1 as filler in LTCS (A333Gr6) welding, particularly in Ammonia service (flash point is minus 33 deg C)?



The working temp is less than minus 33 deg C. At what temp should I impact test it?



Regards,



Nikhil

QC Engineer

Sharjah, UAE

+97150 1453525



--
Click for exclusive coverage on the New Bajaj Pulsar 220 the fastest Indian bike
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...