Saturday, July 25, 2009

[MW:2810] Re: LTCS Welding

E6010 may not be good idea  for low temp application, better use GTAW with ER70S2.
Impact testing temperature shall be your MDMT, not the working temp. check with your designer for MDMT.

BTW pl. don't repeat queries?

On Sat, Jul 25, 2009 at 10:52 AM, Nikhil <nikhilrp_2006@rediffmail.com> wrote:
Dear Friends,

I like to know whether we can use the combination of E6010 in root and E7018-1 as filler in LTCS (A333Gr6) welding, particularly in Ammonia service (flash point is minus 33 deg C)?

The working temp is less than minus 33 deg C. At what temp should I impact test it?

Regards,

Nikhil
QC Engineer
Sharjah, UAE
+97150 1453525



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...