Dear Friends,

I like to know whether we can use the combination of E6010 in root and E7018-1 as filler in LTCS (A333Gr6) welding, particularly in Ammonia service (flash point is minus 33 deg C)?

The working temp is less than minus 33 deg C. At what temp should I impact test it?

Regards,

Nikhil
QC Engineer
Sharjah, UAE