As per ASME Sec II Part A, following is heat treatment requirement about SA 387 (plate material):
"Except for Grades 91 and 91 1, all plates shall be thermally treated either by annealing, normalizing- and - tempering, or, when permitted by the purchaser, accelerated cooling from the austenitizing temperature by air blasting or liquid quenching, followed by tempering"
Code is requesting that plates shall be normalized and tempered, or it shall be normalized-accelerated cooled and tempered (NACT) condition when agreed by the purchaser.
Can anyone guide me what is the difference between "normalizing- and – tempering" plates and "NACT" plates? How it will make difference to the properties of the plates.
For our running project, one of the bidder has said that none of the mill is offering plate in normalizing- and – tempering condition so he has considered NACT condition. Can we accept the plate is NACT condition?
Request to guide me on this topic.
Thanking you,
Sunil Agrawal
Static Equipment Department (STEQU)
--
ARUNVANI
Whatever happened - happened for good; Whatever is happening - is happening for good; Whatever will happen - will happen for good. Do not worry about the past or the future - live in the present.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Friday, July 24, 2009
[MW:2804] Re: Heat treatment of low alloy steel plates SA387 material
Check SA 841.
ARUN
On Fri, Jul 24, 2009 at 8:27 AM, Agrawal Sunil (Mumbai -Stequ) <S.Agrawal@ticb.com> wrote:
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment