[MW:2802] RE: 2797] Heat treatment of low alloy steel plates SA387 material

Check the TT (tempering temperature) in QT steel and NACT steel, the higher TT will increase toughness, but reduce the strength. Generally TT lower in NACT steel in comparison with QT steel.

And when you need PWHT temp below TT, it is difficult to maintain required PWHT below TT when NACT steel are used, ask mill specifically for the temperature(TT) and simulated treatment of test coupons for the specified PWHT temp , include two additional cycles of PWHT.

 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Agrawal Sunil (Mumbai -Stequ)
Sent: 24. juli 2009 09:57
To: materials-welding@googlegroups.com
Subject: [MW:2797] Heat treatment of low alloy steel plates SA387 material

As per ASME Sec II Part A, following is heat treatment requirement about SA 387 (plate material):

 

ā€œExcept for Grades 91 and 91 1, all plates shall be thermally treated either by annealing, normalizing- and - tempering, or, when permitted by the purchaser, accelerated cooling from the austenitizing temperature by air blasting or liquid quenching, followed by temperingā€

 

Code is requesting that plates shall be normalized and tempered, or it shall be normalized-accelerated cooled and tempered (NACT) condition when agreed by the purchaser.

 

Can anyone guide me what is the difference between ā€œnormalizing- and – temperingā€ plates and ā€œNACTā€ plates? How it will make difference to the properties of the plates.

 

For our running project, one of the bidder has said that none of the mill is offering plate in normalizing- and – tempering condition so he has considered NACT condition. Can we accept the plate is NACT condition?

 

Request to guide me on this topic.

 

Thanking you,

Sunil Agrawal

Static Equipment Department (STEQU)





--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...