Wednesday, July 22, 2009

[MW:2777] Re: element reqd. for NACE

Dear PSP

Check it out sulphur content in the material it shd not more than 0.013 for pipe fittings and not more than 0.012 for pipes.

regards

jivan

--- On Wed, 22/7/09, Yadav Shiva <luvshiv2002@gmail.com> wrote:

From: Yadav Shiva <luvshiv2002@gmail.com>
Subject: [MW:2775] Re: element reqd. for NACE
To: materials-welding@googlegroups.com
Date: Wednesday, 22 July, 2009, 12:48 PM


Hi Prashant,
                  Check the Chemical Properties, Mainly the Cromium %
and carbon content.

On 7/22/09, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
> Yes,but which element affects the ordinary material to gain the requirements
> of MR0175.
>
>
> --- On Wed, 22/7/09, Yadav Shiva <luvshiv2002@gmail.com> wrote:
>
>
> From: Yadav Shiva <luvshiv2002@gmail.com>
> Subject: [MW:2771] Re: element reqd. for NACE
> To: materials-welding@googlegroups.com
> Date: Wednesday, 22 July, 2009, 12:13 PM
>
>
>
> Dear prashant ,
>                            please describe what is your requirement
> clearly....  But from my understanding the CS/SS Material should meet
> the NACE Specification MR0175.
> Which service you need?
> On 7/22/09, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
>> Dear all,
>> pl. explain which  element makes the ordinary CS/SS to CS/SS NACE & how?
>> psp
>>
>>
>>       Love Cricket? Check out live scores, photos, video highlights and
>> more. Click here http://cricket.yahoo.com
>> >
>>
>
>
>
>
>
>       Love Cricket? Check out live scores, photos, video highlights and
> more. Click here http://cricket.yahoo.com
> >
>


Love Cricket? Check out live scores, photos, video highlights and more. Click here
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...