Wednesday, July 22, 2009

[MW:2769] RE: 2767] element reqd. for NACE

Hello Prashant,
 
Please read Appendix - F   of ASME 31.3  for your initial understanding.
for NACE consideration precise is para. F323.4.
 
hope it helps.
 
reg
Rahul Pisat
Engineer - Material Engineer
Registered with the trade register of the Chamber of Commerce in Den Haag, The Netherlands, No. 27081325   
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of prashant pansare
Sent: Wednesday, July 22, 2009 8:23 AM
To: mat wel
Subject: [MW:2767] element reqd. for NACE

Dear all,
pl. explain which  element makes the ordinary CS/SS to CS/SS NACE & how?
psp  


Looking for local information? Find it on Yahoo! Local
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...