[MW:2289] RE: 2286] Re: hydro test --- 95% SMYS

 

May 31, 2009

 

Hi,

 

Indirectly the material is cold drawn very slightly during hydrotest at high pressure (90% - 95%SMYS) and becomes stronger. It also follows that there is reduction in the residual stress.

 

Good luck.

PJA

SAVE TREES  - THINK BEFORE YOU PRINT


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Shank Vagal
Sent: Sunday, May 31, 2009 1:36 PM
To: materials-welding@googlegroups.com
Subject: [MW:2286] Re: hydro test

 

Ali.
This is a very unusual query; hydrotest is an integrity test. All other things - where did you get them from?
Rgds
Shank

--- On Sun, 31/5/09, Ali Asghari <asghariali@rocketmail.com> wrote:


From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:2285] hydro test
To: materials-welding@googlegroups.com
Date: Sunday, 31 May, 2009, 9:07 AM

hi

can every body answer two follwing questions?

how hydro test increase the resistance to brittle fracture or failure by crack like flaw?do hydro test decrease residual stress?

 

regard advance.






Cricket on your mind? Visit the ultimate cricket website. Enter now!</a


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...