Sunday, May 31, 2009

[MW:2286] Re: hydro test

Ali.
This is a very unusual query; hydrotest is an integrity test. All other things - where did you get them from?
Rgds
Shank

--- On Sun, 31/5/09, Ali Asghari <asghariali@rocketmail.com> wrote:

From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:2285] hydro test
To: materials-welding@googlegroups.com
Date: Sunday, 31 May, 2009, 9:07 AM

hi
can every body answer two follwing questions?
how hydro test increase the resistance to brittle fracture or failure by crack like flaw?do hydro test decrease residual stress?
 
regard advance.





Cricket on your mind? Visit the ultimate cricket website. Enter now! --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...