Hi

Can you try Furnace brazing with a silver alloyed or copper Shim.
In the past we had successfully brazed a white cast iron to carbon steel by silver alloyed or copper shim by furnace brazing in inert atmosphere.

Regards

Prem Nautiyal
Godrej, Mumbai

On Thu, 28 May 2009 09:15:35 +0530 wrote
>
>I am trying to resistance weld Tungsten Carbide to 420 Stainless
>Steel. Are there any coatings that can enhance the weldabilty of the
>carbide to the stainless steel? Any heat treatings to the steel that
>may help? Currently, it is about 48-52 HRc. We have tried electroless
>nickel on the carbide but would like to be stronger. Any thoughts
>please, Thank you..
>
>>
>

PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...

Pages

Contributors

Blog Archive