Test should be 100% Body and seat but you can witness the test randomly it mean number of valve wise for example out of 100 valve you can witness the test 15 valves Body as well as Seat test.

 

 


On Thu, May 28, 2009 at 12:41 PM, prashant pansare <prashantpan_99@yahoo.co.in> wrote:
Dear all,
I' ve inspected ball & NRV ( API 6D)  valves for xyz company.QAP was not available & client also not provided extent of check,but i inspected Hydro test 100% for body & 10% foe seat & released all the valves after satisfactory results.
My firm wants clarification for Why i not done 100% testing for seat also?
I' ve been warned,badly as i' ve carried out inspection without QAP & taken my own decision.
Is there any specs. or std. to rsolve this matter? & if available pl.forward me,so that i can
responce immediately to avoid further action.
Pl. help.
Regards to all ...PRASHANT    


Explore and discover exciting holidays and getaways with Yahoo! India Travel Click here!



--
TAMIL
phone: +77023210394

 Save a tree...please don't print this e-mail unless you really need toRegards



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...