Hi!

For qualification ,you can qualify on 38mm thk plate.  And weld metal thk should be min 19mm for qualifying max thk for  the particular process . This PQR will qualify to weld partial penetration joint.

 

Regards

 

Hegde

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of PREM SHANKARDUTT NAUTIYAL
Sent: Wednesday, May 27, 2009 9:10 PM
To: materials-welding@googlegroups.com
Subject: [MW:2255] Partial Penetration Joints

 

Hi friends

I need some advice from seniors.

I need to qualify a procedure for a partial penetration joint as per ASME SecIX.
The joint thickness is 56mm, single bevel butt joint. The depth of bevel is only 16mm and thus it is a partial penetration joint.

Now to qualify the WPS/PQR, should i select a 38mm or more thick plate as per QW202.2(b) ??
The statements in QW202.2 are a bit confusing!

Regards

Prem Nautiyal
Godrej, Mumbai.

PREM S NAUTIYAL

CELL : 9820313278

</Table


 


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...