since it is a grrove weld (doesn't matter partial or full penetration), to qualify basemetal (T) you should select 28mm atleast and weld only 8mm to qualify weld metal thickness (t) or full
 
On Wed, May 27, 2009 at 7:40 PM, PREM SHANKARDUTT NAUTIYAL <prem_nautiyal@rediffmail.com> wrote:
Hi friends

I need some advice from seniors.

I need to qualify a procedure for a partial penetration joint as per ASME SecIX.
The joint thickness is 56mm, single bevel butt joint. The depth of bevel is only 16mm and thus it is a partial penetration joint.

Now to qualify the WPS/PQR, should i select a 38mm or more thick plate as per QW202.2(b) ??
The statements in QW202.2 are a bit confusing!

Regards

Prem Nautiyal
Godrej, Mumbai.

PREM S NAUTIYAL

CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...

Pages

Contributors

Blog Archive