dear MALEKAN
it is true.generally the ni content in C-MN steel in weld (or consumable used) shall not be more than 1..5.

 


From: Hamed Malekan <ham_malekan@yahoo.com>
To: materials-welding@googlegroups.com
Sent: Wednesday, May 27, 2009 12:55:29 PM
Subject: [MW:2243] Corrosion in HAZ

I want to know if we weld the material which have below 0.5% Ni with the electrode that contain near about 3% Ni , is there any problem regarding the corrosion in that material . I heard in this case we make the electrolit that in weld metal(Cathod) we have high resistance compare HAZ & corrosion will be more in HAZ & base metal. I want toknow is this idea correct or not.
 
Best Regard

H.Malekan



--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...