I want to know if we weld the material which have below 0.5% Ni with the electrode that contain near about 3% Ni , is there any problem regarding the corrosion in that material . I heard in this case we make the electrolit that in weld metal(Cathod) we have high resistance compare HAZ & corrosion will be more in HAZ & base metal. I want toknow is this idea correct or not.
 
Best Regard

H.Malekan


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...