Saturday, May 23, 2009

[MW:2232] Re: 2225] min and max accepted resiual magnetisum

Rajeev,
Anything in excess of 6 gauss residual magnetism is known to cause problems in welding
such as arc blow.
Rgds,
Shashank Vagal


--- On Sat, 23/5/09, Pablo Acelajado <pjacelajado@npc.com.sa> wrote:

From: Pablo Acelajado <pjacelajado@npc.com.sa>
Subject: [MW:2230] RE: 2225] min and max accepted resiual magnetisum
To: materials-welding@googlegroups.com
Date: Saturday, 23 May, 2009, 2:07 PM

May 23, 2009

 

Dear Rajeev Arora,

 

You must be referring to manganese not magnesium since there is no range or max. for magnesium in API 5L Gr. 70.

 

For Manganese, the range depends on what type of pipe and what WT is involved or whether Seamless, Welded, PSL 1, or PSL 2. For safety you may have a limit of up to 1.4% max for seamless pipe unless otherwise agreed or it could go up to 1.8% for other types. You need to say the type and WT.

 

PJA

 

SAVE TREES  - THINK BEFORE YOU PRINT


From: materials-welding@googlegroups.com [mailto: materials-welding@googlegroups.com ] On Behalf Of rajeev arora
Sent: Friday, May 22, 2009 11:33 AM
To: materials-welding@googlegroups.com
Subject: [MW:2225] min and max accepted resiual magnetisum

 

Dear All,

 

Please give some reference of the max. or range of acceptance of megnetisum in line pipe of API 5L Gr 70.

 

Reagrds

 

Rajeev Arora


--
Regards

Rajeev Arora




"DON'T LET SOMEONE BECOME A PRIORITY IN YOUR LIFE...
WHEN YOU ARE JUST AN OPTION FOR THEM....."

SO , Always keep in mind that......

DON'T GO THE WAY LIFE TAKES YOU,
TAKE THE LIFE THE WAY YOU GO,





Explore and discover exciting holidays and getaways with Yahoo! India Travel Click here! --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...