[MW:2210] Re: Socket Welding


I think the you already received the answer but a groove weld qualification (wpqr/wpq) will cover socket welds too... (see EN 15609/287-1 or ASME IX). 

AJ


Date: Mon, 18 May 2009 22:03:27 +0800
Subject: [MW:2205] Socket Welding
From: kbabupsg@gmail.com
To: materials-welding@googlegroups.com

Hi,
 
Is there any requirement for qualification of Socket welding?

Thanks & regards,

K.Babu
Singapore





Haal meer uit je Hotmail met Internet Explorer 8. Download nu
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...